The invention discloses a door plate suction manufacturing process, which comprises eleven processes of material preparation, material opening, edge moulding of sand edge machine, polishing of sander, router moulding, drilling, line splicing frame moulding, manual inspection grinding, spray drying, sheet parts suction and inspection packaging. The process of making suction doors greatly improves the quality of products, improves the aesthetic level of products, improves production efficiency, does not discharge waste gas and wastewater, and does not cause pollution to the environment. The equipment has an automatic waste recycling device. After waste recycling, it is handled by the government's environmental protection department. The equipment noise in production meets the noise standard of GB12348 industrial enterprise. The production process can effectively reduce the collision damage of production plate in the process of handling and improve the yield of good products.
【技术实现步骤摘要】
一种门板吸塑制造工艺
本专利技术属于家具加工领域,涉及一种柜门加工方法,具体涉及一种门板吸塑制造工艺。
技术介绍
吸塑门是指门板用吸塑材料制成,具有容易擦洗,表面光泽均匀,观感舒适的特点。吸塑模压门是把材质与工艺联合在一起的叫法。“吸”是指真空抽吸的过程;“塑”是指表层的PVC膜;“模”是指刀具铣形后未压PVC膜之前的门板;“压”指的是PVC膜成形时加压的过程,简称为吸塑模压门。现在市场上多数的厂家称之为吸塑门,也有厂家称之为模压门。吸塑门板优点:1、目前,吸塑板是一工程塑料,通过吸塑加工,物理机械性能十分优越,耐冲击性很好,不管是拉伸。弯曲或者压缩强度都很高。而且吸塑板是无定型、无臭无毒的建筑材料。具有良好的耐热性和耐低温性。最低耐寒温度为-60摄氏度,最高耐热温度为120摄氏度。对比原有普通的门性能更加有优势,且更美观,更多元化,使得更多人青睐,生活更加美好。2、吸塑门板外观上木纹逼真且具有立体感,单色色度纯艳,一般不开裂、不变形、耐划、耐热、耐污、防褪色及环保性能好。吸塑门板图案多种多样,经过吸塑模压后能将门板四周封为一体,不需二次封边,解决了有些板材封边后 ...
【技术保护点】
1.一种门板吸塑制造工艺,其特征在于,包括以下步骤:步骤一、备料,包括线条备料和门板备料,线条备料采用窄条的素板,门板备料采用原板材中纤板,并在原板材中纤板单面压贴三聚氰胺纸;步骤二、开料,利用电子锯将单面压贴的中纤板按照设计尺寸进行开料,得到开料好的板材,并在板材上粘贴携带加工信息的二维码;步骤三、砂边机板边造型,根据设计造型调整砂边机刀具,对开料好的板材进行沙边造型;步骤四、砂光机抛光,将板件放置工作台上,通过砂光机将板件表面及棱角进行打磨;步骤五、镂铣做型,利用镂铣机按照设计要求对打磨后的板件进行镂铣造型,之后检测板件纹路和尺寸是否符合要求;步骤六、排钻打孔,板件通过 ...
【技术特征摘要】
1.一种门板吸塑制造工艺,其特征在于,包括以下步骤:步骤一、备料,包括线条备料和门板备料,线条备料采用窄条的素板,门板备料采用原板材中纤板,并在原板材中纤板单面压贴三聚氰胺纸;步骤二、开料,利用电子锯将单面压贴的中纤板按照设计尺寸进行开料,得到开料好的板材,并在板材上粘贴携带加工信息的二维码;步骤三、砂边机板边造型,根据设计造型调整砂边机刀具,对开料好的板材进行沙边造型;步骤四、砂光机抛光,将板件放置工作台上,通过砂光机将板件表面及棱角进行打磨;步骤五、镂铣做型,利用镂铣机按照设计要求对打磨后的板件进行镂铣造型,之后检测板件纹路和尺寸是否符合要求;步骤六、排钻打孔,板件通过三排钻、同心钻进行人工排钻打孔,打孔完成后板件压贴面朝上放置;步骤七、线条裁切及拼框做型,通过45°切割机按照门板尺寸将线条裁切成45°角,将裁切好的线条按照对应的尺寸使用蚊钉枪将线条固定在打孔后的板件上,做成造型;步骤八、检测打磨,人工对拼框做型后的板件半成品进行检查,并对板件进行打磨,用石膏将板件及线条上毛糙、蚊钉孔洞进行磨平,打磨完成后将板件清理干净;步骤九、喷胶烘干处理,将板件平稳放置在待喷胶区域,使用气枪将板件表面清理干净后进行喷胶处理,喷胶完成后的板件进行晾干处理;步骤十、板件吸塑,将晾...
【专利技术属性】
技术研发人员:柯建生,江浩,龚建钊,
申请(专利权)人:索菲亚家居湖北有限公司,