本发明专利技术涉及一种环保无毒粘合剂,以重量份计,包括如下组分:氯化丁基橡胶15‑20份、苍耳粉8‑12份、异氰酸酯10‑12份、环氧氯丙烷5‑16份、聚乙烯醇8‑16份、乳化剂20‑22份、白炭黑3‑8份、脂族聚酯类树脂3‑8份、水20‑25份。本发明专利技术制备工艺简单,制备过程环保无污染,制得的粘合剂粘合效果好,无毒副作用,其挥发物不会污染周围环境,长期使用,对人体无害。

Environmental friendly non-toxic adhesives

The invention relates to an environmentally friendly non-toxic adhesive, which comprises the following components by weight: chlorinated butyl rubber 15 20, Xanthium powder 8 12, isocyanate 10 12, epichlorohydrin 5 16, polyvinyl alcohol 8 16, emulsifier 20 22, white carbon 3 8, aliphatic polyester resin 3 8, water 20 \u3002 The invention has the advantages of simple preparation process, environmental protection and pollution-free preparation process, good adhesive effect, no toxic side effects, no pollution to the surrounding environment, long-term use and no harm to human body.

【技术实现步骤摘要】
环保无毒粘合剂
本专利技术属于材料
,具体涉及一种环保无毒粘合剂。
技术介绍
粘合剂是最重要的辅助材料之一,在包装作业中应用极为广泛。粘合剂定义为可以通过表面粘合及内部强度结合粘附体的非金属材料。粘合剂是具有粘性的物质,借助其粘性能将两种分离的材料连接在一起,粘合剂的种类很多,现有粘合剂气味重,含有有毒物质,粘合效果较差,粘合物品单一,为工业以及家庭等带来不便。
技术实现思路
本专利技术解决其技术问题所采用的技术方案是:一种环保无毒粘合剂,其特征是:以重量份计,包括如下组分:氯化丁基橡胶15-20份、苍耳粉8-12份、异氰酸酯10-12份、环氧氯丙烷5-16份、聚乙烯醇8-16份、乳化剂20-22份、白炭黑3-8份、脂族聚酯类树脂3-8份、水20-25份。本专利技术的有益效果是:本专利技术制备工艺简单,制备过程环保无污染,制得的粘合剂粘合效果好,无毒副作用,其挥发物不会污染周围环境,长期使用,对人体无害。具体实施方式具体实施例:一种环保无毒粘合剂,其特征是:以重量份计,包括如下组分:氯化丁基橡胶15-20份、苍耳粉8-12份、异氰酸酯10-12份、环氧氯丙烷5-16份、聚乙烯醇8-16份、乳化剂20-22份、白炭黑3-8份、脂族聚酯类树脂3-8份、水20-25份。本专利技术的有益效果是:本专利技术制备工艺简单,制备过程环保无污染,制得的粘合剂粘合效果好,无毒副作用,其挥发物不会污染周围环境,长期使用,对人体无害。显然,上述实施例仅仅是为清楚地说明所作的举例,而并非对实施方式的限定。对于所属领域的普通技术人员来说,在上述说明的基础上还可以做出其它不同形式的变化或变动。这里无需也无法对所有的实施方式予以穷举。而由此所引伸出的显而易见的变化或变动仍处于本专利技术创造的保护范围之中。本文档来自技高网...

【技术保护点】
1.一种环保无毒粘合剂,其特征是:以重量份计,包括如下组分:氯化丁基橡胶15‑20份、苍耳粉8‑12份、异氰酸酯10‑12份、环氧氯丙烷5‑16份、聚乙烯醇8‑16份、乳化剂20‑22份、白炭黑3‑8份、脂族聚酯类树脂3‑8份、水20‑25份。

【技术特征摘要】
1.一种环保无毒粘合剂,其特征是:以重量份计,包括如下组分:氯化丁基橡胶15-20份、苍耳粉8-12份、异氰酸酯10-12...