The invention provides a clothing softener which is composed of the following components: nonylphenol polyoxyethylene ether 10 15, sodium hydroxymethylcellulose 3 8, octadecyl dimethylbenzyl ammonium chloride 25 30, magnesium chloride 8 10, tartaric acid 5 8, sodium stearate 15 20, polyvinyl alcohol 15 20, bisphosphoric acid. Sodium hydrogen 8, 10, acrylamide 2, 5, ethanol 30, 40, deionized water 720, 760. The fabric softener of the invention is suitable for cotton and silk fabrics and is convenient to use. After washing and finishing, the cotton and silk fabrics can feel plump, soft and smooth, have elasticity and wear resistance, and the production is convenient and the price is cheap.
【技术实现步骤摘要】
一种衣物柔软剂及其制备方法
本专利技术涉及一种衣物柔软剂及其制备方法。
技术介绍
通常织物在织造、前处理等工艺过程中,很多因素可能使织物变得手感粗糙,均需加柔软剂提高手感。柔软剂是一种能赋予衣物和织物在手感、穿着和使用时有柔软愉悦感觉的产品。柔软剂的平滑、柔软作用主要是由于柔软剂吸附在纤维表面以后,防止纤维与纤维直接接触,降低了纤维与纤维之间的动摩擦系数和静摩擦系数,减少织物组分间的阻力和织物与人体之间的阻力,以达到手感柔软、滑爽、穿着舒适的效果。特别是近年来,柔软剂在纺织品加工中变得尤为重要,几乎每一种从纺织厂出来的纺织品都经过了柔软整理。这种整理的主要目标是获得一种柔软的手感以方便纺织加工和提高穿着性能。通常,令人舒适的柔软手感是顾客在购买一件纺织品时的决定性依据,因此,柔软手感被认为是影响纺织品销售的最重要因素。
技术实现思路
本专利技术提供了一种衣物柔软剂,适用于棉和真丝面料织物。本专利技术提供一种衣物柔软剂,所述衣物柔软剂由以下质量份数的各组分组成:壬基酚聚氧乙烯醚10-15份、羟甲基纤维素钠3-8份、十八烷基二甲基苄基氯化铵25-30份、氯化镁8-10份、酒石酸5-8份、硬脂酸钠15-20份、聚乙烯醇15-20份、磷酸二氢钠。本专利技术还提供上述衣物柔软剂的制备方法,步骤如下:将配方量的壬基酚聚氧乙烯醚、羟甲基纤维素钠、十八烷基二甲基苄基氯化铵、氯化镁、酒石酸、硬脂酸钠、聚乙烯醇混合,加热至70-80℃,搅拌1-2小时,加入配方量的其余组分,搅拌0.5-1小时,冷却至室温即得。本专利技术的衣物柔软剂,适用于棉和真丝面料织物,使用方便,洗涤整理衣物后 ...
【技术保护点】
1.一种衣物柔软剂,其特征在于:所述衣物柔软剂由以下质量份数的各组分组成:壬基酚聚氧乙烯醚10‑15份、羟甲基纤维素钠3‑8份、十八烷基二甲基苄基氯化铵25‑30份、氯化镁8‑10份、酒石酸5‑8份、硬脂酸钠15‑20份、聚乙烯醇15‑20份、磷酸二氢钠8‑10份、丙烯酰胺2‑5份、乙醇30‑40份、去离子水720‑760份。
【技术特征摘要】
1.一种衣物柔软剂,其特征在于:所述衣物柔软剂由以下质量份数的各组分组成:壬基酚聚氧乙烯醚10-15份、羟甲基纤维素钠3-8份、十八烷基二甲基苄基氯化铵25-30份、氯化镁8-10份、酒石酸5-8份、硬脂酸钠15-20份、聚乙烯醇15-20份、磷酸二氢钠8-10份、丙烯酰胺2-5份、乙醇30-40...