The invention discloses a lace dyeing method and lace, including the following steps: step 1: stitching cotton thread onto the nonwoven fabric to sew out the desired shape; step 2: placing the nonwoven fabric in a water bath at 90 110 C for 2 4 hours; out of the vat, weighing, and getting the original product; step 3: placing the original product in the dyeing vat and at the same time. Under the condition of 50 The cotton thread can be sewn on the nonwoven fabric as a medium to easily sew out the desired shape. Then the desired lace can be drawn by using the characteristics that the nonwoven fabric will dissolve at 110 C. The stiff resin can enhance the hardening effect of the initial product and increase the difficulty of loose lace frame after setting.
【技术实现步骤摘要】
一种花边的染色方法及其花边
本专利技术涉及花边织物,特别涉及一种花边的染色方法及其花边。
技术介绍
染料是能使纤维和其他材料着色的物质,随着无纺布的发展,无纺布被越来越多的用于汽车装饰及家居产业,具有颜色的无纺布需求越来越大,且品质要求也越来越多。目前无纺布染料大多采用涂料染色,染出的成品手感粗硬且摩擦色牢度差。公告号为CN102644206B的中国专利公开了一种染色工艺,尤其涉及一种锦涤无纺布的染料染色工艺,包括前处理、染色、固色、拉幅烘干和定型等步骤,所述染色步骤采用染料染色。该专利技术的步骤繁琐,难以在工业上推广,且花边定型困难,容易散架。
技术实现思路
本专利技术的目的是提供一种花边的染色方法,其具有定型稳固,且能够方便,准确地定型出需要的形状。本专利技术的上述技术目的是通过以下技术方案得以实现的:一种花边的染色方法,包括如下步骤:步骤1:将棉线缝合无纺布上;步骤2:将无纺布放置于90-110℃的温度下水浴2-4小时;出缸、称重,得到初品;步骤3:将初品放置于染色缸中并处于50-70℃的条件下,加入染色剂进行染色,持续30-90min后出料;步骤4:将步骤3染 ...
【技术保护点】
1.一种花边的染色方法,其特征是:包括如下步骤:步骤1:将棉线缝合无纺布上;步骤2:将无纺布放置于90‑110℃的温度下水浴2‑4小时;出缸、称重,得到初品;步骤3:将初品放置于染色缸中并处于50‑70℃的条件下,加入染色剂进行染色,持续30‑90min后出料;步骤4:将步骤3染色完毕后的初成品取出,放置于水中,随后按照重量份数,按照硬挺树脂:水=0.5‑1:100的比例加入,浸泡5‑60min,随后取出,定型即可。
【技术特征摘要】
1.一种花边的染色方法,其特征是:包括如下步骤:步骤1:将棉线缝合无纺布上;步骤2:将无纺布放置于90-110℃的温度下水浴2-4小时;出缸、称重,得到初品;步骤3:将初品放置于染色缸中并处于50-70℃的条件下,加入染色剂进行染色,持续30-90min后出料;步骤4:将步骤3染色完毕后的初成品取出,放置于水中,随后按照重量份数,按照硬挺树脂:水=0.5-1:100的比例加入,浸泡5-60min,随后取出,定型即可。2.根据权利要求1所述的一种花边的染色方法,其特征是:按照重量份,棉线与染色剂按照一定比例添加,...