一种球磨端衬板制造技术

技术编号:18297368 阅读:25 留言:0更新日期:2018-06-28 09:19
本实用新型专利技术涉及一种球磨端衬板,包括橡胶衬板和与橡胶衬板相接合的压条,所述压条和所述橡胶衬板的内端面相平齐,所述橡胶衬板为扇形结构,所述橡胶衬板与所述压条依次接合,形成圆形球磨端衬板,消除压条带起钢球冲击衬板的现象,延长了球磨两端衬板的使用寿命,使其寿命延长到7‑8个月,而且还减少了筒体两端附近衬板的磨损情况。

A ball milling end liner

The utility model relates to a ball mill end liner, which comprises a rubber liner and a pressure strip engaged with a rubber liner. The pressure bar is flat with the inner face of the rubber lining board. The rubber lining plate is a sector structure, and the rubber liner joins the pressure strip in turn, forming a circular ball milling end liner and eliminating the steel ball with a strip of pressure. The phenomenon of the impact lining plate prolongs the service life of the lining plate at both ends of the ball mill, prolongs its life to 7 months and 8 months, and also reduces the wear of the liner near the two ends of the barrel.

【技术实现步骤摘要】
一种球磨端衬板
本技术涉及一种球磨端衬板。
技术介绍
矿山单位磨矿阶段绝大多数采用的是球磨机,球磨机端衬板一般材料为锰钢衬板。锰钢衬板更换时费时费力,并且由于衬板重量过大,更换时存在非常大的不安全因素,且锰钢衬板在使用过程中不耐磨,使用周期短,4-5月后经常因为衬板损坏造成停车现象;另外,压条的内端面高于所述端衬板的内端面约10㎝,在磨机运转过中凸出部分能勾带起部分钢球,使钢球的抛落点改变,对筒体两端衬板造成一定冲击,造成筒体两端衬板寿命减少。
技术实现思路
本技术针对上述现有技术中存在的不足,提供一种减少冲击,寿命较长的球磨端衬板。本技术解决上述技术问题的技术方案如下:一种球磨端衬板,包括橡胶衬板和与橡胶衬板相接合的压条,所述压条和所述橡胶衬板的内端面相平齐。进一步,所述橡胶衬板为扇形结构,所述橡胶衬板与所述压条依次接合,形成圆形球磨端衬板。本技术的有益效果是:消除压条带起钢球冲击衬板的现象,延长了球磨两端衬板的使用寿命,使其寿命延长到7-8个月,而且还减少了筒体两端附近衬板的磨损情况。附图说明图1为本技术球磨机筒体端面示意图;图2为图1沿A-A向的剖视图;在附图中,各标号所表示的部件名称列表如下:1、筒体壁,2、橡胶衬板,3、压条。具体实施方式以下结合附图对本技术的原理和特征进行描述,所举实例只用于解释本技术,并非用于限定本技术的范围。如图1-图2所示,一种球磨端衬板,包括橡胶衬板2和与橡胶衬板2相接合的压条3,所述压条3和所述橡胶衬板2的内端面相平齐,所述内端面是指球磨机筒体内部的端面。所述橡胶衬板2为扇形结构,所述橡胶衬板2与所述压条3依次接合,形成圆形球磨端衬板。以上所述仅为本技术的较佳实施例,并不用以限制本技术,凡在本技术的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本技术的保护范围之内。本文档来自技高网...
一种球磨端衬板

【技术保护点】
1.一种球磨端衬板,其特征在于,包括橡胶衬板和与橡胶衬板相接合的压条,所述压条和所述橡胶衬板的内端面相平齐。

【技术特征摘要】
1.一种球磨端衬板,其特征在于,包括橡胶衬板和与橡胶衬板相接合的压条,所述压条和所述橡胶衬板的内端面相平齐。2.根据...

【专利技术属性】
技术研发人员:丁文军王英杰冷守全李春志冷银平孙中建李涛彭剑平付佳杰杜兴乐王林王超
申请(专利权)人:招金矿业股份有限公司蚕庄金矿