一种环保胶粘剂制造技术

技术编号:17437561 阅读:32 留言:0更新日期:2018-03-10 08:17
本发明专利技术公开了一种环保胶粘剂,属于胶粘剂领域。一种环保胶粘剂,包括以下重量份数的组分:环氧丙烷丁基醚5‑15份,邻苯二甲酸二丁酯100‑120份,乳化剂OP-10 40‑50份,10%聚乙烯醇缩甲醛 50‑70份,醋酸乙烯酯20‑30份,氧化铜30‑40份,氢氧化铝30‑40份。本发明专利技术的环保胶粘剂原料易得、制法简单、成本低廉、使用时操作方便,具有含毒小、粘结力强、渗漏性好的优点,环保无污染。

A kind of environmental adhesive

The invention discloses an environmental protection adhesive, which belongs to the field of adhesive. A kind of environment-friendly adhesive, which comprises the following components in parts by weight: butyl epihydrin 5 15 copies, 120 copies of 100 dibutyl phthalate, emulsifier OP 10 40 50, 10% 50 polyvinyl acetate 70, 20 30 copies, 30 copies of 40 copper oxide, aluminum hydroxide 30 40. The environmental protection adhesive has the advantages of easy access, simple manufacturing method, low cost and convenient operation, and has the advantages of small toxicity, strong adhesion and good leakage, and is environment-friendly and pollution-free.

【技术实现步骤摘要】
一种环保胶粘剂
本专利技术涉及胶粘剂领域,具体地说,涉及一种环保胶粘剂。
技术介绍
目前市场上的胶粘剂种类很多,但大多数的胶粘剂中都含有有害物质,容易挥发出来,不仅不利于环保,而且对操作工人的身体也有害。另外,单一性能的胶粘剂不仅性能不好、而且制作工艺复杂、生产成本高、粘结力不强、渗漏性不好。
技术实现思路
本为克服现有技术中存在的技术问题,本专利技术提供一种粘结力强、渗漏性好、制作工艺简单、生产成本低的环保胶粘剂。为解决上述技术问题,本专利技术采用的技术方案如下:一种环保胶粘剂,包括以下重量份数的组分:环氧丙烷丁基醚5-15份,邻苯二甲酸二丁酯100-120份,乳化剂OP-1040-50份,10%聚乙烯醇缩甲醛50-70份,醋酸乙烯酯20-30份,氧化铜30-40份,氢氧化铝30-40份。所述的一种环保胶粘剂的优选配比为:环氧丙烷丁基醚10份,邻苯二甲酸二丁酯110份,乳化剂OP-1045份,10%聚乙烯醇缩甲醛60份,醋酸乙烯酯25份,氧化铜35份,氢氧化铝35份。有益效果本专利技术的环保胶粘剂原料易得、制法简单、成本低廉、使用时操作方便,具有含毒小、粘结力强、渗漏性好的优点,环保无本文档来自技高网...

【技术保护点】
一种环保胶粘剂,其特征在于:包括以下重量份数的组分:环氧丙烷丁基醚5‑15份,邻苯二甲酸二丁酯100‑120份,乳化剂OP-10 40‑50份,10%聚乙烯醇缩甲醛 50‑70份,醋酸乙烯酯20‑30份,氧化铜30‑40份,氢氧化铝30‑40份。

【技术特征摘要】
1.一种环保胶粘剂,其特征在于:包括以下重量份数的组分:环氧丙烷丁基醚5-15份,邻苯二甲酸二丁酯100-120份,乳化剂OP-1040-50份,10%聚乙烯醇缩甲醛50-70份,醋酸乙烯酯20-30份,氧化铜30-40份,氢氧化铝3...

【专利技术属性】
技术研发人员:王军红
申请(专利权)人:南京一禾文化创意有限公司
类型:发明
国别省市:江苏,32

网友询问留言 已有0条评论
  • 还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。

1