Preparation method of preparation method of drug release of termite wood of the invention discloses a drug release anti termite wood, with silica sol, imidacloprid type anti termite emulsion as main raw materials, the first class of imidacloprid termite emulsion into silica sol impregnation, drying under certain pressure. Preparation of drug loaded on termite wood. The invention has abundant raw material resources and low price. The prepared wood has the functions of fireproofing, corrosion prevention, termite protection, etc., and can be widely applied to common wood fields, and has good market application prospect.
【技术实现步骤摘要】
一种载药缓释放防白蚁木材的制备方法
本专利技术涉及一种高比表面积的无机材料,利用载药缓释放作用,填充有机材料,具体涉及一种载药缓释放防白蚁木材的制备方法,属于复合材料领域。
技术介绍
SiO2粉体是一种轻质超细非晶固体物质,是工业中广泛应用的一类补强性填充剂,因密度小、分散性好、高比表面积等特点,对木材、橡胶、塑料的填充增强效果非常好,可吸附药物具有缓释放作用,提高材料的防火、防老化、力学性能。广泛应用于医药、造纸业、纺织业、水处理、胶粘剂、橡胶和塑料填充剂,具有广泛的市场应用价值。如利用纳米SiO2改善淀粉浆料,可以提高浆料耐磨损性能、机械强度和热稳定性。利用硅溶胶浸渍木材,原位填充,可以提高木材的防火性、耐腐蚀性和力学性能。但尚未见有利用SiO2粒子高比表面积吸附作用,制备载药缓释放防白蚁木材的制备方法报道。
技术实现思路
本专利技术的目的是充分利用SiO2粉体具有补强、防火、防腐蚀、吸附等作用,广泛应用于造纸业、纺织业、水处理、胶粘剂、木材、橡胶和塑料填充剂共性,其原材料资源丰富,吸附防白蚁药物缓释放效果显著,有效延长药物作用时间,制备方法简单、价格低廉,具有较 ...
【技术保护点】
一种载药缓释放防白蚁木材的制备方法,其特征在于:是以硅溶胶、吡虫啉类防白蚁乳液为主要原料,先制备载药缓释放防白蚁木材填充原液,通过加压浸渍,干燥得到具有缓释放功能的防白蚁木材。
【技术特征摘要】
1.一种载药缓释放防白蚁木材的制备方法,其特征在于:是以硅溶胶、吡虫啉类防白蚁乳液为主要原料,先制备载药缓释放防白蚁木材填充原液,通过加压浸渍,干燥得到具有缓释放功能的防白蚁木材。2.根据权利要求1所述的一种载药缓释放防白蚁木材的制备方法,其特征在于:将硅溶胶调制成为固体含量为5~40%,加入质量为硅溶胶乳液中固体理论量1~5‰的吡虫啉类防白蚁乳液,搅拌5min~30min,制备载药缓释放防白蚁木材原液。3.根据权利要求1所述的一种载药缓释放防白蚁木材的制备方法,其特征在于:将载药缓释放防白蚁木材原液在30~80℃条件下,0MPa~1.0MPa压力下,浸渍时间为0.5h~10h,浸入硅溶胶与吡虫啉类防白蚁乳液复合原液量为木材质量的10~30%。4.根据权利要求1所述的一种载药缓释放防白蚁木材的制备方法,其特征在于:在100℃温度以下,烘干1h~20h,至恒重,硅溶胶脱水生成SiO2粒子,利用SiO2粒子高比表面积,吸附吡虫啉类防白蚁药物,原位填...