The present invention provides a rubber plastic deodorant, composed of the following components by weight percentage: 18 zeolite 30, tourmaline 5 20 copies, 10 copies, 5 diatomite six ring stone 10 20 copies, 8 copies, 3 calcite shell powder 3 8 and the other is in accordance with the medical stone; the ratio of mixing, high temperature activation, by screening and cooling. The beneficial effect of the invention is the use of natural ore as raw material and deodorant, large adsorption capacity, low cost, in addition to taste lasted for a long time, there is a strong word purification function, there will be no saturation phenomenon, but also has a hygroscopic effect, avoid the use of chemical agents influence people's health. Effective protection of the environment.
【技术实现步骤摘要】
一种橡胶塑料除味剂
本专利技术属于除味剂领域,尤其是涉及一种橡胶塑料除味剂。
技术介绍
在现有的技术中的橡胶塑料除味剂,大部分采用的是活性炭或者其他的有机材料组成,虽然在短时间内有一定的除味效果,但当其本身污染物饱和吸附后,会变成二次污染源,难以持续吸附异味,使用寿命短,治标不治本,会对人体造成一定的伤害。
技术实现思路
本专利技术的目的是针对现有技术存在的不足,提供一种成本低廉、除味效果好、无毒副作用的橡胶塑料除味剂。本专利技术的技术方案是:一种橡胶塑料除味剂,由下述成分按重量百分比组成:沸石18-30份、电气石5-20份、硅藻土5-10份、六环石10-20份、方解石3-8份、贝壳粉3-8份、余量为麦饭石;按照配比混合搅拌、高温活化后,经冷却筛选而成。本专利技术具有的优点和积极效果是:由于采用上述技术方案,采用天然矿石为原料制作的除味剂,吸附量大、成本低廉,除味持续时间长,有很强的字净化功能,不会存在吸附饱和的现象,同时还具有吸湿防潮的作用,避免利用化学试剂影响人们的身体健康,有效的保护了环境。具体实施方式下面结合实施例对本专利技术做详细说明。实施例1本专利技术一种橡胶塑料除味剂,由下述成分按重量百分比组成:沸石30份、电气石5份、硅藻土10份、六环石10份、方解石8份、贝壳粉8份、充分混合后搅拌均匀再加入麦饭石至100份;按照配比混合搅拌、高温活化后,经冷却筛选而成。实施例2本专利技术一种橡胶塑料除味剂,由下述成分按重量百分比组成:沸石22份、电气石10份、硅藻土8份、六环石15份、方解石5份、贝壳粉3份、充分混合后搅拌均匀再加入麦饭石至100份;按照配比 ...
【技术保护点】
一种橡胶塑料除味剂,其特征在于:由下述成分按重量百分比组成:沸石18‑30份、电气石5‑20份、硅藻土5‑10份、六环石10‑20份、方解石3‑8份、贝壳粉3‑8份、余量为麦饭石;按照配比混合搅拌、高温活化后,经冷却筛选而成。
【技术特征摘要】
1.一种橡胶塑料除味剂,其特征在于:由下述成分按重量百分比组成:沸石18-30份、电气石5-20份、硅藻土5-10...
【专利技术属性】
技术研发人员:王颖,
申请(专利权)人:天津日康环保设备有限公司,
类型:发明
国别省市:天津,12