The utility model discloses an automatic Annealers annealing pipe for giant copper core, which comprises a tube body (5), wherein the tube body (5) of the two ends of the nut (2) fixed porcelain head (1); the pipe body (5) is arranged in the hollow ceramic tube (4), (4) the porcelain pipe and the pipe body (5) is arranged between the glass cloth (3). The utility model in order to solve the production line diameter above 3.0mm copper wire can not be oxidized during annealing, vacuum annealing pipe adopts large diameter 76 holes 71, 65, the diameter of ceramic tube also bore 52 large ceramic tube, ceramic head also increased the length of the return tube is thickened and lengthened to 1990mm, so the return the inner hole space not only Datong steam foot vacuum effect and vacuum annealing distance large diameter copper wire annealing up to meet demand of more than 3.0mm, the maximum diameter of the copper wire production line 7.35mm, to fill the gaps in the line annealing on the market.
【技术实现步骤摘要】
一种用于巨型铜芯自动退火机的退火管
本技术涉及到退火机退火系统设计领域,具体来说是一种结构合理的用于巨型铜芯自动退火机退火系统的退火管。
技术介绍
目前市场上的铜线退火机上使用的退火真空管大多是外圆32mm,内孔26mm,长1100mm左右的不锈钢管,只能用于生产线径3.0以下的铜线。铜线在退火机上退火段退火时由于铜线温度急剧升高,如果把温度很高的铜线暴露在空气中铜线就会和空气中的氧气在高温下发生氧化化学作用使铜线氧化变色就会使生产的铜线报废掉,所以为了不让退火的铜线氧化,就让退火温度很高的铜线穿过真空管并往真空管内通入蒸汽而赶走真空管内的氧气,这样就可以避免铜线退火时发生氧化了。但目前市场上铜线退火机真空管外径内孔尺寸及长度都太小过段在生产线径3.0mm以上铜线时由于线径过大真空管小、真空管内蒸汽不多、真空效果不好所以防铜线氧化效果不好,而且大线径铜线容易和真空管内瓷管接触摩擦会划伤铜线表面影响产品质量。因此,在保证铜芯质量的情况下,改进现有的退火管的结构,使其能生产出高质量大直径的铜芯,已经是一个值得研究的问题。
技术实现思路
为了克服上述现有技术中的不足,本技术 ...
【技术保护点】
一种用于巨型铜芯自动退火机的退火管,包括管体(5),其特征在于:所述的管体(5)的两端通过螺母(2)紧固有瓷头(1);所述的管体(5)的内设置有中空的瓷管(4),瓷管(4)与管体(5)中间设置有玻璃丝布(3)。
【技术特征摘要】
1.一种用于巨型铜芯自动退火机的退火管,包括管体(5),其特征在于:所述的管体(5)的两端通过螺母(2)紧固有瓷头(1);所述的管体(5)的内设置有中空的瓷...