一种圆柱镍氢电池制作方法技术

技术编号:16530869 阅读:35 留言:0更新日期:2017-11-09 23:15
本发明专利技术涉及一种圆柱镍氢电池制作方法,用有机聚合物腔水将副隔膜粘在正极片的一端,再将主隔膜置于副隔膜底下,翻折主隔膜,最后将负极片置于主隔膜底下,顺时针卷成一卷,放入电池金属筒内;所述负极片与正极片的长度相同,主隔膜的长度为正极片长度的2倍。本发明专利技术的优点在于:本发明专利技术的方法是用有机聚合物腔水将副隔膜粘在正极片的一端,这样,大批量制作过程副隔膜位置就不易偏离,从而提高电池的质量。

Method for manufacturing cylindrical Ni MH battery

The invention relates to a manufacturing method of a cylindrical Ni MH battery, will stick in the end of the positive plate diaphragm side with the organic polymer water cavity, and then the main separator is arranged under the main folding side diaphragm, diaphragm, the anode sheet is arranged on the main diaphragm under clockwise on a roll, the batteries in the metal tube; the negative plate and a positive plate of the same length, the main diaphragm length is 2 times the length of the positive plate. The invention has the advantages that the method of the invention is to use organic polymer cavity water will stick in the end side of diaphragm, the positive plate so that the mass production process is not easy to deviate from the diaphragm side position, so as to improve the quality of the battery.

【技术实现步骤摘要】
一种圆柱镍氢电池制作方法
本专利技术涉及电池
,尤其涉及一种圆柱镍氢电池制作方法。
技术介绍
圆柱镍氢电池作为一种新型的高性能绿色电池,比镍镉电池的容量高,具有材料新、比能量高、无镉、铅重金属污染和无记忆效应等特点,具有极大的市场容量和广阔的产业化前景。由于圆柱镍氢电池采用正限制,氧化镍正极比容量较低会严重影响电池容量及其他性能指标,所以改进正电极的综合性能尤其是电化学性能是行业的当务之急。圆形圆柱镍氢电池制造包括如下过程:先将活性物质及添加剂等沾附或填充在基带上面做成极片,极片经卷绕制成电池电芯,通过极耳将电芯与壳体或盖帽连接,再经注入电解液、封口等完成,在负极片正极片与隔膜的连接方式上,传统工艺上,一般是在主隔膜上焊一块副隔膜,正极片贴着隔膜,贴着主隔膜另外一面,卷成一个圈放入电池金属筒内。然而大批量制作过程副隔膜位置容易贴偏离,影响电池的质量。
技术实现思路
本专利技术要解决的技术问题是提供一种操作简便、不容易发生质量问题的圆柱镍氢电池制作方法。为解决上述技术问题,本专利技术的技术方案为:一种圆柱镍氢电池制作方法,其创新点在于:用有机聚合物腔水将副隔膜粘在正极片的一端,再将主本文档来自技高网...
一种圆柱镍氢电池制作方法

【技术保护点】
一种圆柱镍氢电池制作方法,其特征在于:用有机聚合物腔水将副隔膜粘在正极片的一端,再将主隔膜置于副隔膜底下,翻折主隔膜,最后将负极片置于主隔膜底下,顺时针卷成一卷,放入电池金属筒内。

【技术特征摘要】
1.一种圆柱镍氢电池制作方法,其特征在于:用有机聚合物腔水将副隔膜粘在正极片的一端,再将主隔膜置于副隔膜底下,翻折主隔膜,最后将负极片置于主隔膜底下,顺时针卷成一卷,放入电池金属筒内...

【专利技术属性】
技术研发人员:曹建民
申请(专利权)人:如皋市下原科技创业服务有限公司
类型:发明
国别省市:江苏,32