The present invention discloses a kind of heavy metal in the livestock and poultry manure targeted removal method, the targeted removal methods include: 1) the attapulgite soaking to sodium silicate aqueous solution, and then adjust the pH to the alkaline surface deposition to prepare silica coated attapulgite; 2) two silicon oxide coating attapulgite, acetone thiosemicarbazone in water by hydrothermal reaction to prepare modified attapulgite; 3) modified attapulgite to filter, then one side of livestock and poultry manure in filter, and then through the water of livestock and poultry manure for directional flushing.
【技术实现步骤摘要】
畜禽粪便中重金属的靶向去除方法
本专利技术涉及重金属去除,具体地,涉及一种畜禽粪便中重金属的靶向去除方法。
技术介绍
随着现代农业的发展,许多国家禽畜养殖业呈现区域化、规模化、专业化、集约化经营的特点,我国也成为一个集约化养殖大国。随着我国畜禽养殖产业的快速发展,畜禽粪便大量产生。禽畜粪便中含有大量的氮、磷等促进农作物生长的元素,禽畜粪便是潜力较大的有机肥源,进过处理后,可用于农业生产,提高土壤肥力、净化生态环境。随着科技的发展,饲料成为了现代养殖产业中禽畜粪便的主要营养来源,饲料的适用在规模化养殖中的一个普遍现象。为了促进禽畜的生长发育,目前,国内大多数企业在饲料中普遍加入了高剂量的铜、锌、硒、砷等重金属元素,一般在全价饲料中铜达到200-300mg/kg,硒达到0.30-0.50mg/kg,作为中国特色的浓缩饲料,其中的铜含量可达1000-1500mg/kg,在1%的预混料中,铜的含量达到2000-3000mg/kg。大量的铜和锌等重金属元素通过新陈代谢循环,一部分沉积在动物体组织中,90%的重金属被排除体外,存留在禽畜粪便中。重金属经过饲料添加——禽畜吸收— ...
【技术保护点】
一种畜禽粪便中重金属的靶向去除方法,其特征在于,所述靶向去除方法包括:1)将凹凸棒土浸泡至硅酸钠水溶液中,然后调节pH至碱性进行表面沉积以制得二氧化硅包覆的凹凸棒土;2)将二氧化硅包覆的凹凸棒土、丙酮缩氨基硫脲于水中进行水热反应以制得改性凹凸棒土;3)将改性凹凸棒土填充至滤网中,接着将畜禽粪便置于滤网的一侧,然后通过水对畜禽粪进行定向冲洗。
【技术特征摘要】
1.一种畜禽粪便中重金属的靶向去除方法,其特征在于,所述靶向去除方法包括:1)将凹凸棒土浸泡至硅酸钠水溶液中,然后调节pH至碱性进行表面沉积以制得二氧化硅包覆的凹凸棒土;2)将二氧化硅包覆的凹凸棒土、丙酮缩氨基硫脲于水中进行水热反应以制得改性凹凸棒土;3)将改性凹凸棒土填充至滤网中,接着将畜禽粪便置于滤网的一侧,然后通过水对畜禽粪进行定向冲洗。2.根据权利要求1所述的靶向去除方法,其特征在于,在步骤1)中,所述凹凸棒土、硅酸钠水溶液的重量比为1:3-6,并且所述硅酸钠水溶液中硅酸钠的浓度为30-41重量%。3.根据权利要求1所述的靶向去除方法,其特征在于,在步骤1)中,所述浸泡至少满足以下条件:浸泡温度为35-55℃,浸泡时间为5-8h。4.根据权利要求1所述的靶向去除方法,其特征在于,在步骤1)中,所述表面沉积的...
【专利技术属性】
技术研发人员:傅剑锋,
申请(专利权)人:安徽乐农环保科技有限公司,
类型:发明
国别省市:安徽,34
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。