The invention relates to an odor paint, including odor emulsion, hydroxyethyl cellulose, fatty acid, coating solvent oil, formaldehyde absorbent, thickening agent, water quality, the number of copies of each component is 27, 12 odor emulsion 10 hydroxyethyl cellulose 18, 15 fatty acids 30, paint solvent oil 6 10, 10, 8 formaldehyde absorbent thickening agent 10 20, water 30 50. Odor paint of the invention is not containing cobalt, lead, used alone, painted light color, good quality, low temperature resistance, high humidity etc.; painted in a variety of architectural surface, quick drying, no sagging, blistering, film formation, has excellent physical and chemical properties, protection, decorative effect good for building up material.
【技术实现步骤摘要】
一种净味涂料
本专利技术涉及一种家装涂料领域,具体地讲,本专利技术涉及一种净味涂料。
技术介绍
普遍存在的油性涂料主要是使用含有大量有毒有害物质的香蕉水、天拿水作为稀释剂,无与伦比的环保优势是水性涂料最大的特点。目前国内外正大力发展水性涂料,随着人们对净味涂料要求的提高,近年来急需在净味涂料生产方法改进上有突破。
技术实现思路
针对现有技术中存在的上述不足,本专利技术所要解决的技术问题是提供一种效果好的净味涂料。本专利技术解决其技术问题所采用的技术方案是:提供一种净味涂料,包括净味乳液、羟乙基纤维素、脂肪酸、涂料溶剂油、甲醛吸收剂、增稠剂、水,各组分的质量份数为:净味乳液12-27、羟乙基纤维素10-18、脂肪酸15-30、涂料溶剂油6-10、甲醛吸收剂8-10、增稠剂10-20、水30-50。作为优选,所述净味涂料各组分的质量份数为:净味乳液23、羟乙基纤维素15、脂肪酸22、涂料溶剂油7、甲醛吸收剂8、增稠剂20、水50。作为优选,所述净味乳液固含量为23-50wt%。作为优选,所述增稠剂为聚丙烯酸酯和聚氨酯的混合物。作为优选,所述水为去离子水。作为优选,所述净味涂料的制备方法,其特征在于包括下述步骤:1)将净味乳液加入搅拌缸中,加入羟乙基纤维素、脂肪酸,搅拌均匀;2)向搅拌缸均匀加入涂料溶剂油,高速搅拌分散;3)均匀加入甲醛吸收剂、增稠剂,搅拌均匀;4)倒入所给质量份数的水,加热20分钟;5)过滤,滤液静置,即可。本专利技术的净味涂料不含钴、铅,单独使用,有漆色浅、质量佳、耐低温、抗高湿等特点;涂于各种建筑表面,干燥迅速、不流挂、不起泡,漆膜平整、具有优 ...
【技术保护点】
一种净味涂料,其特征在于:包括净味乳液、羟乙基纤维素、脂肪酸、涂料溶剂油、甲醛吸收剂、增稠剂、水,各组分的质量份数为:净味乳液12‑27、羟乙基纤维素10‑18、脂肪酸15‑30、涂料溶剂油6‑10、甲醛吸收剂8‑10、增稠剂10‑20、水30‑50。
【技术特征摘要】
1.一种净味涂料,其特征在于:包括净味乳液、羟乙基纤维素、脂肪酸、涂料溶剂油、甲醛吸收剂、增稠剂、水,各组分的质量份数为:净味乳液12-27、羟乙基纤维素10-18、脂肪酸15-30、涂料溶剂油6-10、甲醛吸收剂8-10、增稠剂10-20、水30-50。2.根据权利要求1所述的净味涂料,其特征在于:所述净味涂料各组分的质量份数为:净味乳液23、羟乙基纤维素15、脂肪酸22、涂料溶剂油7、甲醛吸收剂8、增稠剂20、水50。3.根据权利要求2所述的净味涂料,其特征在于:所述净味乳...
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。