The invention relates to an environmental friendly fast drying wood wax oil and a preparation method thereof. The wood wax oil is made of the following raw materials: 50-80 parts by weight of polymerized linseed oil, 6-10 parts by weight of palm wax, 0.5-2.5 parts by weight of beeswax, 5-15 parts by weight of Dama resin, 5-15 parts by weight of d-limonene, 1-4 parts by weight of ascorbyl palmitate, 0.5-2.0 parts by weight of iron isooctanoate and 12-50 parts by weight of anhydrous ethanol. The wood wax oil has the advantages of fast drying speed, low cost, good film-forming performance and no pollution.
【技术实现步骤摘要】
一种环保快干木蜡油及其制备方法
本专利技术涉及一种环保木蜡油,属于木材涂料领域。
技术介绍
近年来世界各国纷纷颁布了严格控制VOC排放量的条例或标准,以限制VOC释放量高的产品的生产和使用。未来涂料向着绿色环保的方向发展是时代的必然选择。天然油蜡涂料统称为木蜡油,其主要是由植物油、动植物蜡、溶剂、助剂等混合而成,是一种类似油漆而又区别于油漆的天然绿色、环境友好型木器涂料,相比于硝基漆、聚氨酯漆等传统木器涂料,木蜡油不含甲醛、苯、甲苯、二甲苯,不含有害VOC、汞、铅、锰、砷等有毒有害的重金属物质。木蜡油的渗透性良好,能充分渗入木材内的管孔中,与木材纤维紧密结合,涂覆于表面不会形成封闭漆膜,不影响木材的自由呼吸,既能增加表面硬度和光泽度,又能起到隔水透气的功能,使木材与空气中水分子实现动态交换平衡,增加木材表面的尺寸稳定性,同时还能起到防虫、防污渍、防酸碱腐蚀等保护作用。木蜡油涂饰木材后,形成极细微的透气式保护表面,不会产生龟裂、脱落、掉漆或斑影的问题,充分其发挥其半开放式的涂装特性,加深木材的天然纹理,赋予木材不同于油 ...
【技术保护点】
1.一种环保快干木蜡油,其特征在于,其是由以下配比的原料制成:/n聚合亚麻油50~80重量份,棕榈蜡6~10重量份,蜂蜡0.5~2.5重量份,达玛树脂5~15重量份,D-柠檬烯5~15重量份,抗坏血酸棕榈酸酯1~4重量份,异辛酸铁0.5~2.0重量份和无水乙醇12-50重量份。/n
【技术特征摘要】
1.一种环保快干木蜡油,其特征在于,其是由以下配比的原料制成:
聚合亚麻油50~80重量份,棕榈蜡6~10重量份,蜂蜡0.5~2.5重量份,达玛树脂5~15重量份,D-柠檬烯5~15重量份,抗坏血酸棕榈酸酯1~4重量份,异辛酸铁0.5~2.0重量份和无水乙醇12-50重量份。
2.如权利要求1所述的环保快干木蜡油,其特征在于,其是由以下配比的原料制成:
聚合亚麻油50~70重量份,棕榈蜡6~10重量份,蜂蜡0.5~2重量份,达玛树脂5~15重量份,D-柠檬烯5~15重量份,抗坏血酸棕榈酸酯1.5~2.5重量份,异辛酸铁0.7~1.5重量份和无水乙醇12-50重量份。
3.如权利要求1或2所述的环保快干木蜡油,其特征在于,所述聚合亚麻油的粘度为3000mpa·s/25℃~5000mpa·s/25℃。
4.一种环保快干木蜡油的制备方法,其特征在于,该方法包括以下步骤:
I.称量聚合亚麻油50~80重量份,棕榈蜡6~10重量份,蜂蜡0.5~2.5重量份,达玛树脂5~15重量份,D-柠檬烯5~15重量份,抗坏血酸棕榈酸酯1~4重量份,异辛酸铁0.5~2....
【专利技术属性】
技术研发人员:黄艳辉,皇权飞,李帆,
申请(专利权)人:北京林业大学,