The embodiment of the application provides a denitration agent and a preparation method thereof, wherein the denitration agent includes: 50 \u2011 65 parts by mass urea, 5 \u2011 10 parts by mass ammonium carbonate, 5 \u2011 10 parts by mass ammonium sulfate, 5 \u2011 10 parts by mass melamine, 5 \u2011 10 parts by mass phenylmelamine, 5 \u2011 10 parts by mass ammonium bicarbonate, 3 \u2011 5 parts by mass magnesium oxide, 1 \u2011 5 parts by mass sodium hypochlorite, 1 \u2011 3 parts by mass Content of bentonite, 1 \u2011 5 content of quicklime and 1 \u2011 3 content of catalyst. The denitration agent provided by the embodiment of the application and the preparation method thereof can solve the problem of high reaction temperature requirements in the conventional denitration scheme.
【技术实现步骤摘要】
脱硝剂及其制备方法
本申请涉及一种脱硝技术,尤其涉及一种脱硝剂及其制备方法。
技术介绍
随着我国化学工业的飞速发展,该领域中的企业数量越来越多,生产规模越来越大,生产过程中排放的废气排放量也逐渐增多。废气中包含有较多的氮氧化物,这是影响空气质量的重要因素。为了避免更多的氮氧化物排放至空气中,通常对废气进行脱硝处理。干法脱硝技术是应用较为广泛的一种方式,是将固体脱硝剂放入反应炉内使其与氮氧化物发生反应,将氮氧化物还原为氮气和水,具有工艺简单、成本低、无废水废弃物排放等优点。在应用过程中,技术人员发现,常规的脱硝剂对反应炉内的温度有较高的要求,必须达到850摄氏度以上,才能达到其最优的反应效率,而保证反应炉的温度达到要求意味着要提高加热功率,进而提高了脱硝成本。
技术实现思路
本申请实施例中提供了一种脱硝剂及其制备方法,能够解决常规脱硝方案中对反应温度要求较高的问题。本申请第一方面实施例提供一种脱硝剂,包括:50-65质量份的尿素、5-10质量份的碳酸铵、5-10质量份的硫酸铵、5-10质量份 ...
【技术保护点】
1.一种脱硝剂,其特征在于,包括:50-65质量份的尿素、5-10质量份的碳酸铵、5-10质量份的硫酸铵、5-10质量份的三聚氰胺、5-10质量份的苯代三聚氰胺、5-10质量份的碳酸氢铵、3-5质量份的氧化镁、1-5质量份的次氯酸钠、1-3质量份的膨润土、1-5质量份的生石灰和1-3质量份的催化剂。/n
【技术特征摘要】
1.一种脱硝剂,其特征在于,包括:50-65质量份的尿素、5-10质量份的碳酸铵、5-10质量份的硫酸铵、5-10质量份的三聚氰胺、5-10质量份的苯代三聚氰胺、5-10质量份的碳酸氢铵、3-5质量份的氧化镁、1-5质量份的次氯酸钠、1-3质量份的膨润土、1-5质量份的生石灰和1-3质量份的催化剂。
2.根据权利要求1所述的脱硝剂,其特征在于,所述催化剂包括:高锰酸钾。
3.根据权利要求1所述的脱硝剂,其特征在于,所述脱硝剂为颗粒状或粉末状。
4.一种权利要求1-3任一项所述脱硝剂的制备方法,其特征在于,包括:
将尿素、碳酸铵、硫酸铵、三聚氰胺、苯代三聚氰胺、碳酸氢铵装入密闭容器内进行搅拌,搅拌持续时间为第一时间段;
加入氧化镁、次氯酸钠...