The invention discloses a modified activated carbon with high efficiency for adsorbing and dearomatizing and its application, which belongs to the field of preparation of activated carbon. The activated carbon is synergistically treated with nitric acid and sulphuric acid, and then filtered and dried to obtain a modified activated carbon capable of selectively adsorbing aromatic amino acids with high efficiency. This kind of activated carbon has a good application in preparing high F value oligopeptides (branched chain amino acid/aromatic amino acid greater than 20). It can greatly reduce the absorption loss of branched chain amino acid by activated carbon, and at the same time can obtain oligopeptide products with high F value. The method has the advantages of simple operation, mild treatment process and high modification efficiency.
【技术实现步骤摘要】
一种高效吸附脱芳的改性活性炭及其制备方法
本专利技术涉及一种高效吸附脱芳的改性活性炭及其制备方法,属于活性炭制备领域。
技术介绍
活性炭是一类良好的吸附剂,因其具有发达的空隙结构和巨大的比表面积,被广泛应用于工业生产许多领域。由于大部分商用活性炭无法满足实际应用,因此需要针对不同的研究对其进行不同方式的改性。改性的方法包括化学改性和物理改性。物理改性是通过改变活性炭的孔径结构以及比表面积,从而提高其吸附量和吸附性能,主要包括高温煅烧和火化等。化学改性是指改变活性炭的表面官能团,来满足对特定物质的选择性吸附,主要包括酸碱改性和氧化改性等。
技术实现思路
本专利技术的目的是利用化学改性得到一种能够良好选择性吸附芳香族氨基酸的活性炭,从而高效制备高F值寡肽产品。为了实现上述目的,本专利技术采用以下技术方案:本专利技术的第一个目的是提供一种制备改性活性炭的方法,所述方法是用HNO3溶液和H2SO4溶液对活性炭进行改性;所述改性是分别用浓度为3~10mol/L的HNO3溶液和浓度为0.1~1mol/L的H2SO4溶液按照固液比为1:5~10的比例浸泡活性炭10~20h,清洗并烘 ...
【技术保护点】
1.一种制备改性活性炭的方法,其特征在于,所述方法是用HNO3溶液和H2SO4溶液对活性炭进行改性;所述改性是分别用浓度为3~10mol/L的HNO3溶液和浓度为0.1~1mol/L的H2SO4溶液按照固液比为1:5~10的比例浸泡活性炭10~20h,清洗并烘干。
【技术特征摘要】
1.一种制备改性活性炭的方法,其特征在于,所述方法是用HNO3溶液和H2SO4溶液对活性炭进行改性;所述改性是分别用浓度为3~10mol/L的HNO3溶液和浓度为0.1~1mol/L的H2SO4溶液按照固液比为1:5~10的比例浸泡活性炭10~20h,清洗并烘干。2.根据权利要求1所述的方法,其特征在于,包括如下步骤:(1)向3~10mol/L的HNO3溶液中以1:5~7的固液比加入颗粒活性炭浸泡10~20h,再清洗至pH5.0~6.0;(2)用0.1~1mol/L的H2SO4溶液以1:5~7的固液比浸泡步骤(1)处理后的活性炭10~20h,而后清洗至pH5.0~6.0,烘干。3.应用权利要求1或2所述方法制备的改性活性炭。4.权利要求3所述的改性活性炭...