The invention discloses a preparation method of polyacrylonitrile fiber textile auxiliaries, which is characterized by weight and consists of 21 parts of organosilicon, 12 parts of octamethyltetrasiloxane, 4.8 parts of sulfonated castor oil, 1.5 parts of hydroxypropyl methyl cellulose, 7 parts of polyvinyl alcohol, 4.5 parts of sodium tripolyphosphate and 1.5 parts of dodecyl sulfuric acid. Sodium, 2 parts magnesium chloride, 9 parts calcium hydrogen phosphate, 1.5 parts 2,3 dihydroxy succinic acid, 1 part triethanolamine. The preparation method of the polyacrylonitrile fiber textile auxiliaries of the invention can make the fabric obtain better softness with small dosage, and has less impact on the environment.
【技术实现步骤摘要】
一种聚丙烯腈纤维纺织助剂的制备方法
本专利技术涉及一种化工制品领域,尤其是涉及一种聚丙烯腈纤维纺织助剂的制备方法。
技术介绍
在洗涤真丝绸、棉绒、针织、府绸等柔软的衣物时,通常的洗衣液只能起到去垢的功效,且目前市面上的柔软剂不能在洗涤整理后达到手感丰满、柔软爽滑、耐磨等诸多性质,使用不是很方便,且柔软剂普遍用量较大,对环境存在较大的影响。
技术实现思路
本专利技术的目的在于提供一种聚丙烯腈纤维纺织助剂的制备方法,该柔软剂具有以交小的用量就能使织物获得较好的柔软性,对环境的影响较小的特点。为了实现上述目的,本专利技术的技术方案是设计一种聚丙烯腈纤维纺织助剂的制备方法,以重量份计,由以下组分组成:21质量份有机硅,12质量份八甲基四硅氧烷,4.8质量份磺化蓖麻油,1.5质量份羟基丙基甲基纤维素,7质量份聚乙烯醇,4.5质量份三聚磷酸钠,1.5质量份十二烷基硫酸钠,2质量份氯化镁,9质量份磷酸氢钙,1.5质量份2,3-二羟基丁二酸,1质量份三乙醇胺。本专利技术的优点和有益效果在于:提供一种聚丙烯腈纤维纺织助剂的制备方法,该柔软剂具有以交小的用量就能使织物获得较好的柔软性,对 ...
【技术保护点】
1.一种聚丙烯腈纤维纺织助剂的制备方法,其特征在于,以重量份计,由以下组分组成:21质量份有机硅,12质量份八甲基四硅氧烷,4.8质量份磺化蓖麻油,1.5质量份羟基丙基甲基纤维素,7质量份聚乙烯醇,4.5质量份三聚磷酸钠,1.5质量份十二烷基硫酸钠,2质量份氯化镁,9质量份磷酸氢钙,1.5质量份2,3‑二羟基丁二酸,1质量份三乙醇胺。
【技术特征摘要】
1.一种聚丙烯腈纤维纺织助剂的制备方法,其特征在于,以重量份计,由以下组分组成:21质量份有机硅,12质量份八甲基四硅氧烷,4.8质量份磺化蓖麻油,1.5质量份羟基丙基...