The invention provides a preparation method of a modified silk fibroin fixing agent, which includes the following steps: washing and drying silk; immersing silk in formic acid aqueous solution and filtering to obtain treated silk; preparing aldehyde solution from glutaraldehyde solution and formaldehyde aqueous solution; immersing the treated silk in aldehyde solution and shaking, adjusting pH, cooling after shaking, washing and drying to prepare modified silk; and preparing LiBr solution. Modified silk protein powder was obtained by centrifugal freeze-drying, laying in the center of the electrode, surface treatment with ammonia, stirring trimethylamine and tetrabutylbromide, dripping epichlorohydrin, heating and stirring, layering and discarding epichlorohydrin, adjusting to pH, diluting with water, adding modified silkworm. Silk protein powder can be obtained by stirring. After fixing silk with fixing agent obtained by this method, the dyeing rate is high, the color fastness to dry and wet rubbing is high, and the color fastness to washing, soaping and fixing is good.
【技术实现步骤摘要】
改性丝素蛋白固色剂的制备方法及其在丝绸固色中的应用
本专利技术涉及改性丝素蛋白固色剂的制备方法及其在丝绸固色中的应用。
技术介绍
丝绸由于具有特有的丝鸣、卓越的悬垂性和良好的光泽,加上穿着轻便舒适,触感缓和柔软,同时吸湿性、透湿性、通气性良好,历来被称为纤维之王。但传统的丝绸染色一般采用酸性染料和媒染染料等染色,染得的丝绸极易褪色,使得丝绸的市场份额一直不大。为了提高丝绸的水洗、皂洗牢度,近年来,对丝绸进行活性染料染色的研究报道增多。用活性染料染丝绸,特别是双活性染料染得的丝绸,水洗牢度可以达到4级、4-5级。但是,由于活性染料在进行分子设计时,为了使得织物染后容易煮浮色,在染料分子中引入了较多的离子基团,使得活性染料极易溶于水。在丝绸染色时,一般上染率、固色率都不高,染料利用率很低。因此,一般都需要使用固色剂,而丝素蛋白与丝绸同宗同源,能够与丝绸更好的结合与匹配,单纯的丝素蛋白并不具备固色效果,因此,需要对其进行改性,提高其固色效果。
技术实现思路
要解决的技术问题:提供一种改性丝素蛋白固色剂的制备方法,所得固色剂对丝绸进行固色后,上染率高,干摩擦和湿摩擦色牢度等级 ...
【技术保护点】
1.改性丝素蛋白固色剂的制备方法,其特征在于:成分按重量份计,包括以下步骤:(1)将5‑10份蚕丝置于含有0.5wt%十二烷基硫酸钠和0.1‑0.2wt%乙醚的水溶液中洗涤,除去杂质,烘干至恒重;(2)按照浴比1:40‑50加入pH值为3.5的甲酸水溶液,常温下浸渍1h,过滤得处理后蚕丝;(3)将200‑250份质量分数为50%的戊二醛溶液、120‑150份30wt%的甲醛水溶液常温混合均匀后,调节pH值至7.5‑8,升温至90℃回流2h;(4)降至室温,用HCl水溶液调节pH值至6‑6.5,在35℃、0.1‑0.2MPa条件下减压蒸馏1h得醛溶液;(5)将处理后蚕丝浸渍于 ...
【技术特征摘要】
1.改性丝素蛋白固色剂的制备方法,其特征在于:成分按重量份计,包括以下步骤:(1)将5-10份蚕丝置于含有0.5wt%十二烷基硫酸钠和0.1-0.2wt%乙醚的水溶液中洗涤,除去杂质,烘干至恒重;(2)按照浴比1:40-50加入pH值为3.5的甲酸水溶液,常温下浸渍1h,过滤得处理后蚕丝;(3)将200-250份质量分数为50%的戊二醛溶液、120-150份30wt%的甲醛水溶液常温混合均匀后,调节pH值至7.5-8,升温至90℃回流2h;(4)降至室温,用HCl水溶液调节pH值至6-6.5,在35℃、0.1-0.2MPa条件下减压蒸馏1h得醛溶液;(5)将处理后蚕丝浸渍于醛溶液中,在40℃恒温水浴摇床上震荡,调节pH值至4,震荡3-4h后冷却,水洗后烘干得改性蚕丝;(6)配制30-40份浓度为9.3M的LiBr溶液,加入改性蚕丝,在温度60-65℃,转速200rpm下搅拌3-4h;(7)倒入透析袋中,用超纯水进行透析,每隔1h换水,10h后变为间隔2-5h换一次超纯水,透析3-4天;(8)取出透析袋,在透析袋表面均匀涂抹PEG20000进行吸水浓缩1-...