The invention discloses a self-healing cement slurry suitable for clastic rock well cementing, which is suitable for the field of petroleum cementing. Its composition is as follows: based on the weight of cement, the percentage of each additive in cement weight is: self-healing agent 5-10%, anti-channeling water loss agent 5-6%, retarder 0.03-0.1%, defoamer 0.1%, water-cement ratio 0.44+0.02, and self-healing agent is dry mixed into cement. At low shear rate, other additive components are mixed with water and wet evenly, and then a certain amount of ash is weighed and added into the slurry mixing liquid, which can be obtained according to the standard slurry mixing. The invention has the advantages of low water loss, adjustable thickening time, excellent anti-gas channeling and impermeability, crack resistance and self-healing functions, and remarkably improves the mechanical properties of cement.
【技术实现步骤摘要】
适用于碎屑岩井固井的自愈合水泥浆
本专利技术涉及油田固井注水泥
,特别涉及一种适用于碎屑岩井固井的自愈合水泥浆。
技术介绍
在油气井作业中,水泥浆主要目的是含填在套管与井壁界面之间的环空中,其作用之一是支撑和保护套管,其二是用于层间分割,因水泥浆凝固、硬化后会形成不渗透水泥石,可以阻止不同层位的流体之间互窜。在我国西部油田,有些区块目的层属于碎屑岩地层,碎屑岩井固井主要是封固产层,产层生产套管固井质量的好坏直接影响到一口井能否顺利交井及后期开采。碎屑岩井地层结构复杂,成岩性差,韧性小、脆性高,地层油水同层、油层水层相隔很近,油水易互窜,难压稳;同时井易漏,难以保证水泥浆返高;该地区采用常规固井施工结束后,CBL测井检测固井质量很好,但射孔压裂时地层出水,验窜地层间封隔不好,还需要进行挤水泥补救,严重影响完井周期。现有的水泥浆体系还不能很好地解决碎屑岩井固井的难题。已公开专利CN102212352A公开了一种防气窜非渗透胶乳固井水泥浆,其组成为100%的水泥和以100%的水泥的重量为基准的降滤失剂2~5%;胶乳稳定剂0.5%~2%;胶乳5%~40%;分散剂0. ...
【技术保护点】
1.一种适用于碎屑岩井固井的自愈合水泥浆,其特征在于,由水泥、自愈合剂、防窜降失水剂、缓凝剂、消泡剂和水组成,以水泥质量为基准,各组分的重量百分比为:水泥100%,自愈合剂5~10%,防窜降失水剂5~6%,缓凝剂0.03~0.1%,消泡剂0.1%,水的加入量满足形成的水泥浆的水灰比为0.44±0.02。
【技术特征摘要】
1.一种适用于碎屑岩井固井的自愈合水泥浆,其特征在于,由水泥、自愈合剂、防窜降失水剂、缓凝剂、消泡剂和水组成,以水泥质量为基准,各组分的重量百分比为:水泥100%,自愈合剂5~10%,防窜降失水剂5~6%,缓凝剂0.03~0.1%,消泡剂0.1%,水的加入量满足形成的水泥浆的水灰比为0.44±0.02。2.根据权利要求1所述的适用于碎屑岩井固井的自愈合水泥浆,其特征在于,所述水泥为G级油井水泥。3.根据权利要求1所述的适用于碎屑岩井固井...
【专利技术属性】
技术研发人员:田宝振,庄建山,孙万兴,宋元洪,和建勇,覃毅,党冬红,陈光,李清洁,刘方义,
申请(专利权)人:中国石油集团渤海钻探工程有限公司,
类型:发明
国别省市:天津,12