The invention discloses a dispensing method which comprises: providing a shell and a panel assembly, providing a shell and a panel assembly, the shell comprises a side wall extending from the bottom wall and the side wall of the bottom wall, the bottom wall and the side wall are surrounded by a groove, an anti-overflow glue is arranged on the inner side of the side wall along the circumference of the side wall, and the anti-overflow glue is solidified to form at least one anti-overflow glue. The panel assembly is set in a groove to seal the gap between the side wall and the edge of the panel assembly; the gap between the top and edge of the side wall is set with sealant; and the solidified sealant is used to fix the connection between the shell and the panel assembly. The dispensing method of the invention can seal the gap between the inner surface and the edge by at least one anti-overflow strip formed by pre-setting and solidifying the anti-overflow glue, and can prevent the filling glue from infiltrating the groove contaminating the shell and/or the panel assembly when the filling glue of the solidified shell and the panel assembly is subsequently set. The invention also provides an input and output component and an electronic device.
【技术实现步骤摘要】
点胶方法、输入输出组件及电子装置
本专利技术涉及电子装置,尤其涉及一种点胶方法、输入输出组件及电子装置。
技术介绍
在相关技术中,手机等电子装置包括壳体和面板组件,壳体形成有凹槽,面板组件设置凹槽中,壳体与面板组件的侧面一般通过点胶的方式的固定连接。然而,由于胶水具有流动性,胶水容易流至面板组件的底部污染面板组件。
技术实现思路
本专利技术提供一种点胶方法、输入输出组件及电子装置。本专利技术实施方式的点胶方法包括步骤:提供壳体和面板组件,所述壳体包括底壁和自所述底壁的侧边延伸的侧壁,所述底壁与所述侧壁围成有凹槽;沿所述侧壁的周向在所述侧壁的内侧上设置防溢胶水;固化所述防溢胶水以形成至少一个防溢条;将所述面板组件设置在所述凹槽,所述防溢条密封所述侧壁和所述面板组件的边缘之间的缝隙;在所述侧壁的顶部和所述边缘之间的所述缝隙设置填缝胶水;和固化所述填缝胶水以固定连接所述壳体和所述面板组件。本专利技术实施方式的输入输出组件包括壳体、面板组件、至少一个防溢条和填缝胶条。所述壳体包括底壁和自所述底壁的侧边延伸的侧壁,所述底壁与所述侧壁围成有凹槽。所述防溢条通过沿所述侧壁的周向在所述侧壁的内侧上设置防溢胶水并固化形成。所述面板组件设置在所述凹槽。所述防溢条密封所述侧壁和所述面板组件的边缘之间的缝隙。填缝胶条通过在所述侧壁的顶部和所述边缘之间的所述缝隙设置填缝胶水并固化形成。所述填缝胶条固定连接所述壳体和所述面板组件。本专利技术实施方式的电子装置包括本体和以上任一实施方式的输入输出组件。所述输入输出组件设置在所述本体上。本专利技术实施方式的点胶方法、输入输出组件和电子装置通过 ...
【技术保护点】
1.一种点胶方法,其特征在于,包括以下步骤:提供壳体和面板组件,所述壳体包括底壁和自所述底壁的侧边延伸的侧壁,所述底壁与所述侧壁围成有凹槽;沿所述侧壁的周向在所述侧壁的内侧上设置防溢胶水;固化所述防溢胶水以形成至少一个防溢条;将所述面板组件设置在所述凹槽,所述防溢条密封所述侧壁和所述面板组件的边缘之间的缝隙;在所述侧壁的顶部和所述边缘之间的所述缝隙设置填缝胶水;和固化所述填缝胶水以固定连接所述壳体和所述面板组件。
【技术特征摘要】
1.一种点胶方法,其特征在于,包括以下步骤:提供壳体和面板组件,所述壳体包括底壁和自所述底壁的侧边延伸的侧壁,所述底壁与所述侧壁围成有凹槽;沿所述侧壁的周向在所述侧壁的内侧上设置防溢胶水;固化所述防溢胶水以形成至少一个防溢条;将所述面板组件设置在所述凹槽,所述防溢条密封所述侧壁和所述面板组件的边缘之间的缝隙;在所述侧壁的顶部和所述边缘之间的所述缝隙设置填缝胶水;和固化所述填缝胶水以固定连接所述壳体和所述面板组件。2.如权利要求1所述的点胶方法,其特征在于,所述凹槽大致呈矩形,所述侧壁包括长侧壁和连接所述长侧壁的短侧壁,所述沿所述侧壁的周向在所述侧壁的内侧上设置防溢胶水的步骤包括以下步骤:沿所述长侧壁的长度方向在所述长侧壁的内侧上设置所述防溢胶水。3.如权利要求2所述的点胶方法,其特征在于,所述沿所述长侧壁的长度方向在所述长侧壁上设置所述防溢胶水的步骤包括以下步骤:沿所述长侧壁的长度方向在所述长侧壁的内侧连续地设置所述防溢胶水。4.如权利要求1所述的点胶方法,其特征在于,所述防溢胶水包括硅酮胶。5.如权利要求1所述的点胶方法,其特征在于,所述固化所述防溢胶水以形成至少一个防溢条的步骤包括以下步骤:在20-25℃的环境中固化所述防溢胶水超过五分钟。6.如权利要求1所述的点胶方法,其特征在于,所述防溢胶水的固化时间小于所述防溢胶水的完全固化时间。7.如权利要求1所述的点胶方法,其特征在于,所述凹槽大致呈矩形,所述侧壁包括内侧面,所述内侧面包括长侧面和连接所述长侧面的短侧面,所述短侧面形成有台阶,所述台阶包括台阶面、连接所述台阶面及所述长侧面的阶下面和连接所述台阶面的阶上面,所述沿所述侧壁的周向在所述侧壁的内侧上设置防溢胶水的步骤包括以下步骤:沿所述阶下面的长度方向连续地设置所述防溢胶水。8.如权利要求7所述的点胶方法,其特征在于,所述将所述面板组件设置在所述凹槽的步骤包括以下步骤:在所述台阶面上设置粘接胶水;将所述面板组件支撑在所述台阶面上;和固化所述粘接胶水以粘接所述台阶面和所述面板组件。9.如权利要求1所述的点胶方法,其特征在于,所述面板组件包括触控面板和覆盖在所述触控面板上的盖板,所述盖板的横向尺寸大于所述触控面板的横向尺寸以使所述边缘在所述盖板和所述触控面板之间形成阶梯面,所述边缘包括盖板边缘和触控面板边缘,所述在所述侧壁的顶部和所述边缘之间的所述缝隙设置填缝胶水的步骤包括以下步骤:在所述侧壁的顶部和所述盖板边缘之间的缝隙设置所述填缝胶水;所述固化所述填缝胶水以固定连接所述壳体和所述面板组件的步骤包括:固化所述填缝胶水以固定连接所述壳体和所述盖...
【专利技术属性】
技术研发人员:侯康,曾武春,周国安,向韬,
申请(专利权)人:广东欧珀移动通信有限公司,
类型:发明