The invention discloses a fir fast drying method, which comprises the following steps: the wood cut sheet; sheet formation will be discharged to the drying kiln, bar is arranged between each layer of wood bunch drying kiln; close the door, the kiln for heating, and to maintain constant temperature; moisture content for the plate, stop heating, room temperature to drop naturally, the sheet to sheet out of the kiln; drying, the moisture content of wood until qualified. The beneficial effect of the invention is that the moisture content in wood can be removed quickly, the stability of wood can also be improved, the larger deformation amount will be avoided, and the quality of products will be improved.
【技术实现步骤摘要】
一种杉木快速干燥方法
本专利技术涉及一种木材处理方法,特别涉及一种杉木快速干燥方法。
技术介绍
杉木,不仅是自然景观中的奇葩,也是建筑装饰的良材。由于其颜色协调统一,常用于制作精细木家具、高档家具,在软木胶合镶板的夹层、木铲和造纸业中也有广泛的应用,其它用途包括:单板、木结构框架、灯具、抽屉侧板、室内施工、成套家具、桌子、箱柜、护壁板和车削制品。
技术实现思路
本专利技术的目的在于克服现有技术中所存在的上述不足,提供一种杉木快速干燥方法。为了实现上述专利技术目的,本专利技术提供了以下技术方案:一种杉木快速干燥方法,包括如下步骤:(1)将木材锯切成5-8cm厚的板材;(2)将板材平整排放于烘干窑内,材堆的每层木板之间设置隔条,格条高度为10-20cm;(3)关闭干燥窑门,对窑内进行加热升温至80-120°,并保持恒温48-72小时;(4)待板材含水率在10-20%时,停止加热,待室温自然下降至20-30°时,将板材出窑;(5)待板材自然风干,直至木材含水率合格。与现有技术相比,本专利技术的有益效果:快速去除木材中的水分,还能提高木材的稳定性能,避免其出现较大变形量,有利 ...
【技术保护点】
一种杉木快速干燥方法,其特征在于, 包括如下步骤:(1)将木材锯切成5‑8cm厚的板材;(2)将板材平整排放于烘干窑内,材堆的每层木板之间设置隔条,格条高度为10‑20cm;(3)关闭干燥窑门,对窑内进行加热升温至80‑120°,并保持恒温48‑72小时;(4)待板材含水率在10‑20%时,停止加热,待室温自然下降至20‑30°时,将板材出窑;(5)待板材自然风干,直至木材含水率合格。
【技术特征摘要】
1.一种杉木快速干燥方法,其特征在于,包括如下步骤:(1)将木材锯切成5-8cm厚的板材;(2)将板材平整排放于烘干窑内,材堆的每层木板之间设置隔条,格条高度为10-20cm;(3)关闭干燥窑门...
【专利技术属性】
技术研发人员:黄开满,
申请(专利权)人:四川美登家具有限公司,
类型:发明
国别省市:四川,51