The invention relates to a soil acidification improver and its preparing method, the compositions of raw materials according to the weight proportion is composed of the following: Obsidian 10 15 copies, 15 copies, 10 lime coconut shell activated carbon 6 12 copies, 5 shell powder 10 copies, 11 copies, 6 thatrhc nano silica solution 6 10 copies, 30 copies, 25 alfalfa carboxymethyl cellulose 6 8 mg 3, sugar alcohol 5, 6, 4 zinc glycine 5 10 microbial strains. The material of the invention is easy, safe and non-toxic, alfalfa through microbial fermentation, effectively improve the activity, can kill harmful bacteria and protect bacteria, can promote the permeability of soil, loosen the soil, reduce the loss of nutrients, improve the structure, improve the soil acidity, ensure stable in neutral pH, increase the content of organic matter. Improve soil water, accelerate plant growth speed.
【技术实现步骤摘要】
一种土壤酸化改良剂及其制备方法
本专利技术涉及土壤改良剂领域,具体涉及一种土壤酸化改良剂及其制备方法。
技术介绍
由于工业的发展,酸性气体排放量增加,酸雨量逐年增加导致土壤酸化越来越严重,土壤酸化是指土壤吸收性复合体接受了一定数量交换性氢离子或氯离子,使土壤中碱性离子流失的过程,导致PH值降低,形成酸性土壤,影响土壤中生物活性,改变养分心态,降低有效性,进而使游离的金属离子融入土壤溶液中,对作物产生毒害,所以土壤酸性化的改变势在必得。
技术实现思路
本专利技术的目的是为了克服以上的不足而提供一种土壤酸化改良剂及其制备方法。本专利技术的技术方案包括:一种土壤酸化改良剂及其制备方法,原料组成成分按重量份数由以下比例组成:黑曜岩10-15份、生石灰10-15份、椰壳活性炭6-12份、贝壳粉5-10份、稻壳炭6-11份、纳米二氧化硅溶液6-10份、苜蓿25-30份、羧甲基纤维素6-8份、糖醇镁3-5份、甘氨酸锌4-6份、微生物菌种5-10份。本专利技术的进一步改进在于:其制备方法如下:A、常温常压下,将黑曜岩和生石灰进行打粉,混合物椰壳活性炭和稻壳炭进行搅拌,搅拌速率为580 ...
【技术保护点】
一种土壤酸化改良剂及其制备方法,其特征在于:原料组成成分按重量份数由以下比例组成:黑曜岩10‑15份、生石灰10‑15份、椰壳活性炭 6‑12份、贝壳粉5‑10份、稻壳炭6‑11份、纳米二氧化硅溶液6‑10份、苜蓿25‑30份、羧甲基纤维素6‑8份、糖醇镁3‑5份、甘氨酸锌4‑6份、微生物菌种5‑10份。
【技术特征摘要】
1.一种土壤酸化改良剂及其制备方法,其特征在于:原料组成成分按重量份数由以下比例组成:黑曜岩10-15份、生石灰10-15份、椰壳活性炭6-12份、贝壳粉5-10份、稻壳炭6-11份、纳米二氧化硅溶液6-10份、苜蓿25-30份、羧甲基纤维素6-8份、糖醇镁3-5份、甘氨酸锌4-6份、微生物菌种5-10份。2.根据权利要求1所述的一种土壤酸化改良剂及其制备方法,其特征在于:其制备方法如下:A、常温常压下,将黑曜岩和生石灰进行打粉,混合物椰壳活性炭和稻壳炭进行搅拌,搅拌速率为5...