The utility model discloses a powder diffusion device for continuously preparing high silicon steel thin strip, comprising a steel belt conveying device (4), transmission device (19) and two (27) steel belt conveying device composed of assembly line, strip conveying device (4) is provided with a front (spray pill machine 3), shot peening machine (3) low silicon steel strip winding mechanism is arranged in front of the steel belt conveying device (1); (4) and a transmission device (19) is arranged between the two cathode roller (5, 15), two (5, 15 cathode roller) is arranged between the powder diffusion furnace (10) in the transmission device; (19) and two (27) strip conveying device of a heat treatment furnace is arranged between the two conveying device (24); strip (27) is arranged behind the high silicon steel belt winding mechanism (28). The utility model has the advantages of simple operation, low temperature silicon increasing operation, low cost, and continuous preparation of large size near final high silicon steel strip.
【技术实现步骤摘要】
一种粉末扩散法连续制备高硅硅钢薄带的装置
本技术涉及一种磁场下连续制备高硅钢薄带的装置,属于磁性材料制备、热处理
技术介绍
硅钢薄带是一种非常重要的软磁材料,广泛应用于电力、电器以及国防军事工业等领域中。当硅钢薄带中硅含量增加到6.5wt%后,硅钢的磁致伸缩趋近于零,综合磁性能达到最佳,是高频磁性元件用的理想软磁材料。但是,当硅含量超过4wt%后,随着硅含量的增加,脆性显著增加,当硅含量增加到5wt%以后,硅钢的延伸率近乎降低至零。因此,很难采用传统的轧制和冲压加工法制备高硅硅钢薄带。目前为止,世界各国研究人员对6.5wt%Si高硅硅钢薄带的制备方法进行了大量研究,并提出了多种制备工艺,如激光熔敷喷涂法、粉末轧制法、熔盐电沉积法、CVD法、PCVD法、多道轧制法、复合电沉积-扩散法等。目前日本的NKK公司开发的化学气相沉积法即CVD法生产的6.5wt%Si硅钢薄带具备很好的磁性能,并已小规模进行工业化生产,但存在对设备要求高、铁流失严重、沉积温度高、能耗大、硅钢表面质量差、污染环境、成本高等缺点,限制了其进一步大规模化生产。当采用复合电镀热处理法制备高硅 ...
【技术保护点】
一种粉末扩散法连续制备高硅硅钢薄带的装置,其特征在于:包括由钢带输送装置一(4)、传送装置(19)和钢带输送装置二(27)构成的流水作业线,在钢带输送装置一(4)的前方设有喷丸机(3),喷丸机(3)的前方设有低硅钢带卷绕机构(1);钢带输送装置一(4)和传送装置(19)之间设有两个阴极夹辊(5、15),两个阴极夹辊(5、15)之间设有粉末扩散炉(10),粉末扩散炉(10)上下两面由内而外依次设有加热装置一(9)、绝热材料一(8)、水冷装置一(7)和恒定磁场发生器一(6);粉末扩散炉(10)中设有上阳极(12)、下阳极(13)以及热电偶一(14);粉末扩散炉(10)下方设有控 ...
【技术特征摘要】
1.一种粉末扩散法连续制备高硅硅钢薄带的装置,其特征在于:包括由钢带输送装置一(4)、传送装置(19)和钢带输送装置二(27)构成的流水作业线,在钢带输送装置一(4)的前方设有喷丸机(3),喷丸机(3)的前方设有低硅钢带卷绕机构(1);钢带输送装置一(4)和传送装置(19)之间设有两个阴极夹辊(5、15),两个阴极夹辊(5、15)之间设有粉末扩散炉(10),粉末扩散炉(10)上下两面由内而外依次设有加热装置一(9)、绝热材料一(8)、水冷装置一(7)和恒定磁场发生器一(6)...
【专利技术属性】
技术研发人员:伍玉娇,龙琼,黄芳,凌敏,周登凤,路坊海,何杰军,李杨,
申请(专利权)人:贵州理工学院,
类型:新型