The utility model discloses a cloth crack as building material, including the base cloth layer, on both sides of the base cloth layer by layer were stuck to the table cloth and oily paper, the elastic coefficient of fabric layer is larger than the elastic coefficient of surface layers, such as building material cloth crack, can avoid the table cloth for wall the cracking of the stretch and tear, greatly increase the surface layers of life, prolong the using time of the cloth crack, compared with the existing elastic structure for anti crack material zero or weak, it can hold long time increase the reaction force of the wall, delaying the wall cracking stress release, the wall is not easy to crack, other construction when only the oily paper, and then the base cloth layer can be affixed to the wall, simple operation and good construction environment.
【技术实现步骤摘要】
一种用作建筑材料的防裂布
本技术涉及建筑装修材料领域,特别是指一种用作建筑材料的防裂布。
技术介绍
传统墙体的接缝施工中,需采用以白乳胶、石膏、粘粉、白水泥、化学接缝剂(如环氧树脂接缝剂)等材料为原料的混合浆进行填充找平,然后贴上玻纤网、牛皮纸带、橡胶带或草带等防裂材料结构,如此,以增加墙体的反应力作用,延缓墙体开裂的应力释放,使墙体不容易开裂或进一步地开裂。然而,上述所述的防裂材料结构,其弹性大都为零或较弱,在墙体受天气影响产生热胀冷缩、或因地基沉降位移而释放应力,预开裂或逐步出现轻微裂纹的过程中,墙体释放的应力过大,大于防裂材料结构内部应力时,防裂材料结构则易被撕裂,影响其寿命,对墙体的防裂作用也不复存在。且现有防裂材料结构的粘贴大都采用上述冷胶技术,即将混合浆涂刷于墙体表面,而后将防裂布平整地铺于墙体上进行贴合。该种粘贴技术,粘贴过程繁琐、不环保,特别是,施工完成后,若再次出现裂缝,需将原有接缝处固化后的混合浆清理干净,再重复上述工艺施工,施工过程会产生大量粉尘及大面积的建筑垃圾。
技术实现思路
本技术的目的是提供一种用作建筑材料的防裂布。实现本技术目的的技术方案是,一种用作建筑材料的防裂布,包括基布层,基布层的两侧通过胶层分别贴置有表布层和油性纸,基布层的弹性系数大于表布层的弹性系数。进一步地,表布层的弹性系数为零。以便防裂布具有较强的坚韧性,确保增加墙体的反应力作用。进一步地,极限拉伸状态下,单位长度的基布层具有1~2倍单位长度的形变量。该种基布层,既不会因弹性系数过大而丧失防裂作用,又不会因弹性系数过小,墙体开裂时,无法产生大的形变,致使过渡至表布 ...
【技术保护点】
一种用作建筑材料的防裂布,包括基布层,其特征在于:基布层的两侧通过胶层分别贴置有表布层和油性纸,基布层的弹性系数大于表布层的弹性系数。
【技术特征摘要】
1.一种用作建筑材料的防裂布,包括基布层,其特征在于:基布层的两侧通过胶层分别贴置有表布层和油性纸,基布层的弹性系数大于表布层的弹性系数。2.根据权利要求1所述的用作建...