Using starch as reinforcing agent for corrugated paper, by the number of copies of the following raw materials: corn starch consists of 25 ~ 35, 15 ~ 25 copies of purple sweet potato starch, sodium sulfate, 10 to 20 portions of glutinous rice amylopectin 20 ~ 25, 15 ~ 20 copies of soda ash and hawthorn acid 25 - 35, fatty alcohol polyoxyethylene ether 2 - 4, 2 - 4 of p-nitrobenzoic acid, four boric acid sodium 1 - 2, two methyl maleic anhydride 2 ~ 3, 10 ~ 15 modified oxidizing agent, deionized water, starch of the invention enhances the bonding performance of corrugated reinforcing agent, and meet the carton board will not spread, avoid hardening carton board, moisture-proof performance, water will not fail.
【技术实现步骤摘要】
一种瓦楞纸用淀粉增强剂
本专利技术涉及淀粉施胶剂
,具体涉及一种瓦楞纸用淀粉增强剂。
技术介绍
瓦楞纸箱粘箱需要使用施胶剂,施胶剂是具有粘性的物质,借助其粘性能将两种分离的材料连接在一起。施胶剂的种类很多。目前大都使用淀粉施胶剂,但是目前的施胶剂总存在一些问题,严重影响着瓦楞纸箱粘箱。
技术实现思路
本专利技术要解决的技术问题是提供瓦楞纸用淀粉增强剂:本专利技术的瓦楞纸用淀粉增强剂增强了粘结性能,而且遇到纸箱板不会扩散,避免了纸箱板的硬化,防潮性能好,遇水不会失效。为实现上述技术目的,达到上述技术效果,本专利技术通过以下技术方案实现:一种瓦楞纸用淀粉增强剂,由以下份数的原料组分组成:玉米淀粉25~35份、紫薯淀粉15~25份、硫酸钠10~20份、糯米支链淀粉20~25份、纯碱15~20份、山楂酸25~35份、脂肪醇聚氧乙烯醚2~4份、对硝基苯甲酸2~4份、四硼酸钠1~2份、改性氧化剂10~15份、去离子水若干。优选的,还可由以下份数的原料组分组成:玉米淀粉30份、紫薯淀粉20份、硫酸钠15份、糯米支链淀粉23份、纯碱18份、山楂酸30份、脂肪醇聚氧乙烯醚3份、对硝基苯甲酸3份、四硼酸钠1份、改性氧化剂13份、去离子水若干。优选的,所述改性氧化剂由以下重量份的原料制成:月桂醇聚氧乙烯醚硫酸钠5~12份、红矾钠6~1份、过氧化月桂酰3~5份、没食子酸钙2~5份、过氧化氢对孟烷4~12份、椰油酰胺丙基甜菜碱8~12份。一种瓦楞纸用淀粉增强剂,制备方法如下:(1)将上述质量份数的去离子水加热到70~85℃,然后将上述质量份数的玉米淀粉、紫薯淀粉、硫酸钠、糯米支链 ...
【技术保护点】
一种瓦楞纸用淀粉增强剂,其特征在于:由以下份数的原料组分组成:玉米淀粉25~35份、紫薯淀粉15~25份、硫酸钠10~20份、糯米支链淀粉20~25份、纯碱15~20份、山楂酸25~35份、脂肪醇聚氧乙烯醚2~4份、对硝基苯甲酸2~4份、四硼酸钠1~2份、改性氧化剂10~15份、去离子水若干。
【技术特征摘要】
1.一种瓦楞纸用淀粉增强剂,其特征在于:由以下份数的原料组分组成:玉米淀粉25~35份、紫薯淀粉15~25份、硫酸钠10~20份、糯米支链淀粉20~25份、纯碱15~20份、山楂酸25~35份、脂肪醇聚氧乙烯醚2~4份、对硝基苯甲酸2~4份、四硼酸钠1~2份、改性氧化剂10~15份、去离子水若干。2.根据权利要求1所述的瓦楞纸用淀粉增强剂,其特征在于:由以下份数的原料组分组成:玉米淀粉30份、紫薯淀粉20份、硫酸钠15份、糯米支链淀粉23份、纯碱18份、山楂酸30份、脂肪醇聚氧乙烯醚3份、对硝基苯甲酸3份、四硼酸钠1份、改性氧化剂13份、去离子水若干。3.根据权利要求1所述的...
【专利技术属性】
技术研发人员:刘祥鹏,
申请(专利权)人:安徽凤凰松包装有限公司,
类型:发明
国别省市:安徽,34