The invention discloses a process for producing a concave heat transfer film, which comprises the following steps: first use of foaming ink in film printing; secondly, many local printing accumulation raised in need raised position; then printing after oven heating and drying after foaming foaming, convex reach bump height design requirements; also included on the foaming and drying after surface coating printing adhesive, bump touch surface the accumulation and production of foam combination, smoothness controllable product, and saves ink, fast drying, and finally through the method of the heat transfer system with concave handle ceiling or wall.
【技术实现步骤摘要】
一种凹凸热转印膜的生产工艺以及一种吊顶或墙板的制造方法
本专利技术属于热转印
,具体地说是涉及一种凹凸热转印膜的生产工艺以及一种吊顶或墙板的制造方法。
技术介绍
具有凹凸手感表面的产品具有强烈的触觉感官以及视觉上的立体感,在吊顶、墙纸、集成墙板等家居装饰以及其他行业深受消费者的喜爱,但是现在常用的生产方法就是采用多层油墨印刷来堆积出局部的凸起,这种方法堆积层较厚不但浪费油墨,而且干燥速度缓慢,直接导致生产成本高,效率低;还有采用发泡油墨印刷后直接进行发泡产生凸起,这种方法经常会出现发泡量不足而无法达到预期凹凸效果。
技术实现思路
本专利技术的目的是提供一种凹凸热转印膜的生产工艺以及一种吊顶或墙板的制造方法,其采用堆积和发泡相结合进行凹凸手感表面生产,产品的凹凸量可控,并且节省油墨,干燥速度快。为解决上述技术问题,本专利技术的目的是这样实现的:一种凹凸热转膜的生产工艺,包括以下步骤:A、在薄膜上使用发泡油墨进行印刷;B、在需要凸起的位置进行多次印刷堆积出局部凸起;C、印刷后经过烘箱进行加温发泡和干燥,发泡后局部凸起达到设计要求的凸起高度;在上述方案的基础上并作为上 ...
【技术保护点】
一种凸凹热转膜的生产工艺,其特征在于包括以下步骤:A、先在薄膜表面涂离型剂形成透明脱离层;B、在透明脱离层上使用普通油墨进行印刷;C、在需要凸起的位置使用发泡油墨进行印刷堆积出局部凸起;D、印刷后经过烘箱进行加温发泡和干燥,发泡后局部凸起达到设计要求的凸起高度。
【技术特征摘要】
1.一种凸凹热转膜的生产工艺,其特征在于包括以下步骤:A、先在薄膜表面涂离型剂形成透明脱离层;B、在透明脱离层上使用普通油墨进行印刷;C、在需要凸起的位置使用发泡油墨进行印刷堆积出局部凸起;D、印刷后经过烘箱进行加温发泡和干燥,发泡后局部凸起达到设计要求的凸起高度。2.根据权利要求1所述的一种凸凹热转膜的生产工艺,其特征在于:步骤A所述薄膜为PET膜。3.根据权利要求1所述的一种凸凹热转膜的生产工艺,其特征在于:步骤C之后还包括对发泡和干燥后的印刷物表面涂布粘合剂。4.根据权利要求3所述的一种凸凹热转膜的生产工艺,其特征在于:所述涂布粘合剂选用100-140...
【专利技术属性】
技术研发人员:赵忠祥,
申请(专利权)人:海宁市恒康塑料包装有限公司,
类型:发明
国别省市:浙江,33
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。