The invention discloses a method for processing Roushi tile pollution, which comprises the following steps: (1) preparation of concentration of acetic acid mixed solution of 3 10%; (2) using the above steps (1) on tile pollution sites were fully wet acetic acid mixed solution prepared by acetic acid and calcium hydroxide to produce pollution substances neutralization reaction, chemical reaction formula is as follows: 2CH3COOH+Ca (OH) = 2 = Ca (CH3COO) 2+2H2O; (3) using plastic brush wash tile pollution site, rinse with water. The processing method effectively reduced the labor intensity of workers, and improve the efficiency, save a lot of time; facing bricks and treated with excellent gloss and color retention, waterproof performance, greatly prolong the service life of Roushi decorative brick.
【技术实现步骤摘要】
一种处理柔石饰面砖污染的方法
本专利技术涉及墙面清理
,尤其涉及一种处理柔石饰面砖污染的方法。
技术介绍
针对前面被污染的情况,现有处理被污染墙面的方法是把受污染墙面用自来水充分湿润后,再用软棕毛刷洗污染部位,刷完后再用干净自来水冲洗受污染洗刷部位墙面,直到被污染部位干净为止。上述现有处理技术一般轻微的污染能处理干净,但比较严重的就处理不干净或不彻底了,因柔石饰面砖本身是建材的材料属性,故现场墙面污染大部分都是墙体里硅酸盐水泥水化反应后渗透出来的氢氧化钙(化学式Ca(OH)2)白色结晶物质,即墙体泛碱物质。当以上原因造成的污染源比较厚或已结痂时,软棕毛刷由于本身过软,对已结痂到一定硬度的氢氧化钙(化学式Ca(OH)2)泛碱污染物刷不掉或刷不干净,另自来水也不能和氢氧化钙(化学式Ca(OH)2)产生直接反应,而只起到了冲洗洗刷后残留物的效果,以上2个原因造成现有方法对严重污染墙面处理得不干净或不彻底,导致产品外观颜色看起来不逼真。针对被污染的柔石饰面砖的清理存在较大提升空间,因此,急需一种操作简单、清理干净彻底且能够还原墙面原色效果的处理方法,以解决上述污染墙 ...
【技术保护点】
一种处理柔石饰面砖污染的方法,其特征在于,包括如下步骤:(1)配制浓度为3‑10%的乙酸混合溶液;(2)采用上述步骤(1)制得的乙酸混合溶液对饰面砖污染部位进行充分湿润,使乙酸与污染源物质氢氧化钙产生酸碱中和反应,化学反应式如下:2CH3COOH+Ca(OH)2==Ca(CH3COO)2+2H2O;(3)采用塑料刷洗刷饰面砖污染部位,用水冲洗干净即可。
【技术特征摘要】
1.一种处理柔石饰面砖污染的方法,其特征在于,包括如下步骤:(1)配制浓度为3-10%的乙酸混合溶液;(2)采用上述步骤(1)制得的乙酸混合溶液对饰面砖污染部位进行充分湿润,使乙酸与污染源物质氢氧化钙产生酸碱中和反应,化学反应式如下:2CH3COOH+Ca(OH)2==Ca(CH3COO)2+2H2O;(3)采用塑料刷洗刷饰面砖污染部位,用水冲洗干净即可。2.根据权利要求1所述的处理柔石饰面砖污染的方法,其特征在于,所述步骤(1)中配制乙酸混合溶液的浓度为5%。3.根据权利要求1所述的处理柔石饰面砖污染的方法,其特征在于,所述步骤(3)中塑料刷采用硬质塑料刷。4.根据权利要求1所述的处理柔石饰面砖污染的方法,其特征在于,还包括对步骤(3)用水冲洗干净后的墙面喷涂40-50℃的外墙防护剂。5.根据权利要求1所述的处理柔石饰面砖污染的方法,其特征...
【专利技术属性】
技术研发人员:陈国迈,陈迈华,卓为民,张云生,姚慧,
申请(专利权)人:上海古猿人石材有限公司,
类型:发明
国别省市:上海,31