The invention discloses a four sided elastic leather base cloth, which is made of spandex or Leica and other flat low elastic silk yarn as warp yarn and woven into elastic fabric. The fabric is made to make leather base cloth after dyeing and finishing. The thickness of the base plate to Maojian is 1.2 and 2.5 millimeters, one of which is arranged in one side, and the yarn in the yarn is spandex according to the weight percentage. The content is 6, 9%, and the other components are 91 - 94%. The four side elastic leather base cloth of the invention has good elasticity, high preparation method and stable quality of weaving products.
【技术实现步骤摘要】
一种四面弹革基布及其制备方法
:本专利技术涉及纺织领域,具体讲是一种四面弹革基布及其制备方法。
技术介绍
:现有的弹革基布弹力不好,限制了弹革基布的运用范围。
技术实现思路
:本专利技术所要解决的技术问题是,提供一种弹性好的四面弹革基布。本专利技术的技术解决方案是,提供一种四面弹革基布,采用氨纶或莱卡与其它成分的扁平低弹丝的纱作为经纱,织成弹力坯布,坯布经染整后制得革基布;所述革基布的底版到毛尖的厚度为1.2-2.5毫米,其中一面设有绒;按重量百分比,纱中氨纶含量为6-9%,其它成分的纤维为91-94%。本专利技术所要解决的另一技术问题是,提供一种四面弹革基布的制备方法,包括下列步骤:a,坯布织造,b,染色定型,其中,坯布织造包括以下步骤,(1)原料采购;(2)纱线整经;(3)织机织造形成坯布;染色定型包括以下步骤,(1)卧式定型机进行坯布定型,卧式定型机速度为:35±2m/分钟温度为:185-195±2℃;(2)起毛机起毛;(3)烫光;(4)剪毛;(5)染色,染色温度为:125±2℃,速度为:95±2m/min;(6)色坯定型;(7)烫光;(8)成品。本专利技术与现有技术相比,具有以下有益效果,织造的四面弹革基布弹性好,染色色不会褪色,织造效率高,产品质量稳定。具体实施方式:下面就具体实施方式对本专利技术作进一步说明:一种四面弹革基布,采用氨纶或莱卡与其它成分的扁平低弹丝的纱作为经纱,织成弹力坯布,坯布经染整后制得革基布;所述革基布的底版到毛尖的厚度为1.2-2.5毫米,其中一面设有绒;按重量百分比,纱中氨纶含量为6-9%,其它成分的纤维为91-94%。其中 ...
【技术保护点】
一种四面弹革基布,其特征在于:采用氨纶或莱卡与其它成分的扁平低弹丝的纱作为经纱,织成弹力坯布,坯布经染整后制得革基布;所述革基布的底版到毛尖的厚度为1.2‑2.5毫米,其中一面设有绒;按重量百分比,纱中氨纶含量为6‑9%,其它成分的纤维为91‑94%。
【技术特征摘要】
1.一种四面弹革基布,其特征在于:采用氨纶或莱卡与其它成分的扁平低弹丝的纱作为经纱,织成弹力坯布,坯布经染整后制得革基布;所述革基布的底版到毛尖的厚度为1.2-2.5毫米,其中一面设有绒;按重量百分比,纱中氨纶含量为6-9%,其它成分的纤维为91-94%。2.一种四面弹革基布的制备方法,其特征在于,包括下列步骤:a,坯布织造,b,染色定型,其...